It's not hard to make the 3d liquid floors in the bathroom, but the effect will be simply stunning. The bathroom will change just before your eyes, the color variation chosen for your taste will not only visually increase the room, but also make it inimitable. But I advise you to turn to the professionals of Mega-Comfort Ltd. liquid floors 3 D. The whole process will take only four days, and the effect will be simply stunning.

3d floor is a coating consisting of several layers. A three-dimensional image is located under the transparent polymeric layer. Consider how to make 3d liquid floors in the bathroom itself in four days.

The first day

First, you need to prepare the foundation. As a rule, the floor in the bathroom is concrete. The base must be cleaned of dirt, remove dust. The prepared surface should be primed. For this purpose, for example, epoxy primer duroglass FF-4416. These primers consist of two components, which should be thoroughly mixed with a drill with a paddle stirrer for about two minutes. The finished mixture is applied to the substrate with a velor roller. The primer freezes for thirty minutes. The consumption of this material is from 0.25 to 0.35 kilograms per square meter and depends on the condition of the surface being treated.

Second day

The surface to be primed should be leveled. To do this, the epoxy base coat Duroglass 5/2 is used. - A different color RAL. These components have in their composition two components: a hardener and a resin additive. With a layer thickness of two millimeters, the material consumption will be about one and a half kilograms per square meter. The manufacturer of the mixture usually points to the packaging of the recipe for cooking. Stirring is carried out with a drill. Finished putty poured onto the frozen primer and spreads evenly with a spatula throughout the floor area.

It is recommended to carry out this work in special shoes with studded soles to avoid leaving traces.

Day Three

At this stage, the cleanliness of the surface of the cured putty should be given great attention, since it will be glued to the 3d image. A picture can be any. You can find it on the Internet or order a design in an advertising agency (Buy 3 d images here). The main condition is high image quality. It should also be taken into account that the 3d effect, as a rule, is developed for a certain position with which a person will look.

The picture is printed on banner paper in a printing or advertising agency. When ordering, remember a small margin along the edges of the image. Trimming the picture should be done on the spot. Banner fabric is glued to the base on a thin layer of the finish floor. The image is smoothed by the roller. Under the banner cloth, there should be no air bubbles.

Day four

The final stage is the application of a polymer coating - the finish layer. Two components of the polymer material (EPD-127) should be thoroughly mixed. At a thickness of three millimeters, the flow rate will be 3.5-4 kilograms per square meter.

On the pasted image the prepared mixture pours out. Using a spatula or roller, the polymer coating is distributed throughout the area evenly. For 15-30 minutes before starting, pierce the solution with a needle roller.

Self-leveling 3D floors are ready. Walk on the polymer can be after two or three days. Completely the same 3d floor will be ready for loads of days in five to seven.